Material No. | 2.4619 |
---|---|
EN symbol (short) | NiCr22Mo7Cu |
AISI/SAE | G-3 |
UNS | N 06985 |
AFNOR | — |
B.S. | — |
alloy | alloy G-3 |
Registered work's label | Inconel® G-3, Nicrofer® 4823hMo, Hastelloy®alloy G-3 |
Standards | — |
Material 2.4619 (alloy G-3) is a chemically stable and high-temperature resistant alloy, which is well weldable and has a good stability against grain border corrosion in welded condition. Alloy 2.4619 (alloy G-3) is used in flue gas scrubbers, and with phosphoric and sulphuric acid.
Our product range in 2.4619 (alloy G-3) are tubes and pipes, fittings and flanges, accessories.
Chemical composition ¹ | ||||||||
C ≤ % | Si ≤ % | Mn ≤ % | P ≤ % | S ≤ % | Cr % | Mo % | Ni % | V % |
0,015 | 1,5 | 1,0 | 0,025 | 0,015 | 21,0-23,5 | 6,0-8,0 | rest | |
Nb ² % | Ti % | Al % | Co ≤ % | Cu % | N % | Fe % | Ce % | W ≤ % |
0,5 | 5,0 | 1,5-2,5 | 18,0-21,0 | 1,5 | ||||
¹ in accordance with Key to Steel 2001 ² Nb+Ta |
Special characteristics | ||
Temperature range | Density kg/dm³ | Hardness |
---|---|---|
annealed typically up to 600° | 8,14 |
Welding filler |
covered rod electrode 2.4621 |
Main fields of application (depending on the specific conditions of use) |
flue gas scrubbers, chemical industry, phosphoric acid, sulphuric acid, acetic acid, petrochemical plants, production of fertilisers |
(all aforementioned specifications serve as a general orientation and have to be reviewed depending on the specific conditions of use) |